Chloorkop, Kempton Park · Gauteng Mon–Thu 05:30–15:30 · Fri 05:30–12:00

Insights · 15 September 2026 · 6 min read

EN8 vs EN19 vs EN24: choosing the right engineering steel

Use EN8 for lightly loaded shafts and pins, EN19 for most stressed shafts and gears, and EN24 when the section is large or the load is heavy or shock-type. EN19 and EN24 are close to AISI 4140 and 4340.

Short answer: EN8 is a plain medium-carbon steel for lightly to moderately loaded parts. EN19 is a chromium-molybdenum steel, usually supplied hardened and tempered, for stressed shafts, gears and pins. EN24 is a nickel-chromium-molybdenum steel for heavily loaded or shock-loaded parts and larger sections. EN19 is close to AISI 4140 and EN24 is close to AISI 4340.

As toolmakers and machinists, we cut all three every week. The right choice depends on load, section size, whether the part needs hardening, and how much machining it needs. The guide below sets out how we think about it.

The EN designations in brief

The EN numbers come from the old British Standard BS 970. That standard was replaced by European standards years ago, but EN8, EN19 and EN24 are still the names most South African engineers, buyers and steel merchants use.

Grade BS 970 designation Alloy type Closest common equivalents
EN8 080M40 Medium-carbon, unalloyed C40 / C45, AISI 1040 / 1045
EN19 709M40 Chromium-molybdenum 42CrMo4 (1.7225), AISI 4140
EN24 817M40 Nickel-chromium-molybdenum 34CrNiMo6 (1.6582), AISI 4340

All three have roughly 0.4% carbon. The difference is the alloying. EN19 adds chromium and molybdenum. EN24 adds nickel as well. Those additions raise hardenability, meaning how deep into a section the steel will harden when quenched. That is why EN24 keeps its strength in thicker bars than EN19, and EN19 in thicker bars than EN8.

What condition T and condition V mean

BS 970 used letter codes for tensile strength ranges after hardening and tempering. You will still see them on drawings and mill certificates.

Condition Typical tensile range Typical hardness (indicative)
R 700–850 MPa approx. 201–255 HB
T 850–1000 MPa approx. 248–302 HB
V 1000–1150 MPa approx. 293–352 HB

Two points matter in practice:

  • The condition only holds up to a limiting section size. A large-diameter bar cannot always reach the same core strength as a small one. EN24 holds condition T in larger diameters than EN19 does. For big sections, check the ruling section on the material certificate.
  • The values are typical, not guaranteed. Always confirm actual tensile strength and hardness from the material certificate supplied with the bar.

Typical properties compared

The figures below are typical, indicative values for bar in common conditions. Use them for an early comparison only, and design to the certificate.

EN8 EN19 EN24
Usual supply condition As-rolled or normalised Hardened and tempered, condition T Hardened and tempered, condition T (also V)
Typical tensile strength approx. 550–700 MPa (normalised) approx. 850–1000 MPa (T) approx. 850–1000 MPa (T); 1000–1150 MPa (V)
Toughness Moderate Good Very good, including at low temperature
Through-hardening Poor in larger sections Good in moderate sections Very good in large sections
Machinability Good Fair to good in T Fair in T; harder in V
Weldability Fair with preheat Difficult; needs a procedure Difficult; generally avoided
Relative cost Lowest Medium Highest

EN8: the general-purpose choice

EN8 is the workhorse for parts that do not see high stress. It machines well, it is easy to get, and it is the cheapest of the three.

Typical uses:

  • Lightly loaded shafts, spindles and axles
  • Pins, studs, bolts and keys
  • Bushes, spacers and collars
  • Brackets and general machine parts

EN8 can be flame or induction hardened. That gives a hard, wear-resistant surface on journals or bearing seats while the core stays tougher. It does not through-harden well in larger sections, so do not expect alloy-steel core strength from a large EN8 bar.

EN8D is a variant often used where better machinability or consistency is needed. Check which one your drawing calls for.

EN19: the stressed-part standard

EN19 is the steel we recommend most often for shafts, gears and pins that carry real load. It is usually bought pre-hardened and tempered to condition T. That means the part can be machined straight from bar and put into service without further heat treatment.

Typical uses:

  • Drive shafts, pinion shafts and gearbox shafts
  • Gears, sprockets and couplings
  • High-tensile pins, bolts and studs
  • Hydraulic and pneumatic components
  • Tooling holders and machine parts that need a tough core

EN19 responds well to nitriding and to induction hardening. That makes it a good choice where a hard, wear-resistant surface is needed over a strong core, for example on a shaft running in a bush.

EN24: for heavy loads and large sections

EN24 earns its higher price when the part is large, heavily loaded or exposed to shock and fatigue. The nickel content improves toughness and lets the steel harden more deeply. In thick sections it holds its strength better than EN19.

Typical uses:

  • Heavy-duty shafts, axles and crankshafts
  • Large gears and gear blanks
  • Mining and earthmoving components that see shock loads
  • Highly stressed pins, bolts and connecting rods
  • Parts that need higher conditions such as V or above

EN24 in condition V is noticeably harder to machine than in condition T. It wears tools faster and needs slower, more rigid cutting. Factor that into cost and lead time when specifying it.

Heat treatment and machining sequence

For most EN19 and EN24 work, buying pre-hardened bar in condition T is simpler and cheaper than hardening after machining. It avoids distortion and scale on finished parts.

Where higher hardness is needed, the usual route is:

  1. Rough machine the part, leaving stock on critical diameters and faces.
  2. Heat treat to the required hardness, or nitride or induction harden the wearing surfaces.
  3. Finish machine or grind critical dimensions after heat treatment, so distortion is corrected.

Precision fits, bearing seats and seal faces are often finished by surface or cylindrical grinding after hardening. Heat treatment specifications, temperatures and quench media should be set by the designer or the heat treater for the specific part.

When to use 4140 or 4340 equivalents

Many drawings from overseas equipment makers specify AISI 4140 or 4340, or European grades such as 42CrMo4 and 34CrNiMo6. In South Africa, EN19 and EN24 are usually the practical substitutes.

  • 4140 or 42CrMo4 on the drawing: EN19 is the normal local equivalent.
  • 4340 or 34CrNiMo6 on the drawing: EN24 is the normal local equivalent.

The chemistries are close but not identical. For general machine parts the substitution is routine. For safety-critical, pressure-retaining or certified components, confirm the substitution with the original designer, and specify the condition or hardness you need rather than just the grade.

Availability in South Africa

EN8, EN19 and EN24 are widely stocked by South African steel merchants in round bar, with EN19 and EN24 most commonly supplied in condition T. Flat bar, very large diameters, other conditions such as V, and some European or American grades may need to be ordered in. That can add time to a job, so tell us early if your drawing specifies something unusual.

Our practical rule of thumb

  • Low stress, no shock, cost matters: EN8.
  • Real torque or bending, moderate section, wants a tough core: EN19 in condition T.
  • Heavy, shock or fatigue loading, or a large section: EN24.
  • Needs a hard wearing surface: EN8 induction hardened for light duty, or EN19 or EN24 nitrided or induction hardened for higher loads.

If you are unsure, send us the drawing or the worn part with a note on how it is used. We will suggest a material and condition that suits the job, and explain the trade-off on cost. We turn, mill and grind all three grades in our toolroom in Chloorkop, Kempton Park. See CNC turning and CNC milling, or request a quote.

Frequently asked questions

Is EN19 the same as 4140?

They are close equivalents rather than identical specifications. EN19 (709M40) and AISI 4140 are both chromium-molybdenum steels with around 0.4% carbon, and EN19 is the usual South African substitute when a drawing calls for 4140 or 42CrMo4. For safety-critical parts, confirm the substitution with the designer.

What does condition T mean on EN19 or EN24?

Condition T is a tensile strength band from the old BS 970 system, typically 850 to 1000 MPa. It tells you the bar has been hardened and tempered to that range, so it can be machined and used without further heat treatment.

Can EN24 be welded?

Only with care. EN24 has high hardenability, so welding without the right preheat, controlled cooling and post-weld heat treatment risks cracking. Where possible, design EN24 parts so they do not need welding, or get a welding procedure qualified first.

Should I use EN8 or EN19 for a shaft?

If the shaft is lightly loaded and not subject to shock, EN8 is usually adequate and cheaper. If it carries significant torque, bending or shock loads, or needs a hardened and tempered core, EN19 in condition T is the more reliable choice.

Can EN8 be hardened?

Yes. EN8 can be flame or induction hardened to give a hard, wear-resistant surface on journals and bearing seats, and it can be hardened and tempered. Because it is unalloyed, it does not through-harden well in larger sections.

Is EN24 always better than EN19?

No. EN24 is stronger and tougher in large sections but it costs more and is harder to machine. For many moderately stressed parts, EN19 does the same job at lower cost.

Keep reading

More guides

29 Sep 2026 · 6 min read

Repair or replace a worn blow mould? A practical decision guide

Most blow mould wear on pinch-offs, parting lines, cavity edges and neck inserts can be repaired by micro welding, re-machining and re-polishing. Replacement makes sense when sealing faces or threads are badly worn, damage recurs, or the repair would cost more downtime than a new part.

22 Sep 2026 · 6 min read

What to send for an accurate machining quote

For an accurate machining quote, send a 3D STEP file and a dimensioned 2D PDF drawing, plus the material and condition, quantity and repeat volumes, finish, critical tolerances and required delivery date.

WhatsApp us